ASTM A268 Tubes

Standard Specification for Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service 










Table 1 Chemical Requirments 

Grade  TP405 TP410 TP429 TP430 TP443 TP446-1 TP446-2A ... TP409 TP439
UNS Designation S40500 S41000 S42900 S43000 S44300 S44600 S44600 S40800 S40900 S43035 
Element  Composition, % 
C, Max 0.08 0.15 0.12 0.12 0.20 0.20

0.12

0.08 0.08 0.07
Mn, Max 1.00 1.00 1.00 1.00 1.00 1.50 1.50 1.00 1.00 1.00
P, Max 0.040 0.040 0.040 0.040 0.040 0.040 0.040 0.045 0.045 0.040
S, Max 0.030 0.030 0.030 0.030 0.030 0.030 0.030 0.045 0.030 0.030
Si, Max 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00
Ni 0.50 max ... ... ... 0.75 max 0.75 max 0.50 max 0.80 max 0.50 max 0.50 max
Cr 11.5-14.5 11.5-13.5 14.0-16.0 16.0-18.0 18.0-23.0 23.0-27.0 23.0-27.0 11.5-13.0 10.5-11.7 17.0-19.0
Mo ... ... ... ... ... ... ... ... ... ...
Al 0.10-0.30 ... ... ... ... ... ... ... ... 0.15
Cu ... ... ... ... 0.90-1.25 ... ... ... ... ...
N ...



0.25 0.25

0.04
Ti ...





12XC Min;1.10 max 6XC min; 0.75 max 0.20+4(C+N)min;1.10 max 

A For small diameter or thin walls, or both, tubing, where many drawing passes are required, a carbon maximum of 0.015 % is necessary. Small outside diameter tubes are defined as those less than 0.500 in. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 in. [1.2 mm] in average wall thickness (0.040 in. [1 mm] in minimum wall thickness). 


1, General Requirements

Material furnished under this specification shall conform to the applicable requirements of Specification A1016/A1016M unless otherwise provided herein.


2, Manufacture

The tubes shall be made by the seamless or welded process with no filler metal added. 











3, Surface Condition

All tubes shall be free of excessive mill scale, suitable for inspection. A slight amount of oxidation will not be

considered as scale. Any special finish requirements shall be subject to agreement between the manufacturer and the purchaser.


4, Mechanical Tests Required 

1) Tension Tests

2) Flange Test (for Welded Tubes) (For tubes over 8 in. [203.2 mm] in outside diameter, or tubes with wall thickness 3⁄8 in. [9.52 mm] and over, the flattening test may be performed instead of the flange test unless the flange test is specified in the purchase order.)

3) Hardness Test 

4) Reverse Flattening Test 


MW Metal offers both Eddy current test and air underwater test for 100% tubes. 










Back
Previous Product:DIN EN 10312 Welded Tubes
Next Product:ASTM A270 TUBES

About us

Profile Vision&Mission Our Strength Images Industry We Serve

Inhouse Manufacturing

Outsource Manufacturing

Downloads

International Standards Dimensions Specifications

Links

Packing & Marking Global Network Manufacturing Process Flow Chart
Copyright 2019 MW Metal Industry